Novel Glass Fibre Z-Pins to Improve the Delamination Bridging Performance of Laminated Composite Materials

Novel Glass Fibre Z-Pins to Improve the Delamination Bridging Performance of Laminated Composite Materials

Romain RUTAR, Luiz KAWASHITA, Eduardo SANTANA DE VEGA, Christophe BOUVET, Bruno CASTANIÉ, Stephen R HALLETT

Abstract. Laminated composite stiffened panels are sensitive to impact-induced interlaminar damage, which can drastically diminish their strength. Z-pinning can help overcoming this issue by preventing delamination propagation. Among other, impact induces local mode II driven fracture, for which industry standard carbon fibre (CF) Z-pins perform poorly. This study exploits on the superior failure strain of S2-glass (GF) fibres to develop Z-pins that maintain effectiveness across a full spectrum of mode mixities. The 0.3mm diameter GF/epoxy pins are produced via in-house micro-pultrusion. To explore the impact of fibre diameter, two distinct configurations, 9µm and 14µm diameter fibres, are considered. These GF-based pins are then benchmarked against industry standard carbon fibre T300/BMI pins. Additionally, in order to separate the contributions of the fibre and that of the resin, T300/epoxy pins are manufactured through the same micro-pultrusion process. Z-pinned samples are loaded across the whole range of mode mixities using a miniature Arcan setup. S2-glass’ superior compliance and failure strain delay the transition from Mode I pullout to mode II fibre rupture for GF pins compared to CF pins. Furthermore, in the event of GF pins rupture under mode II loading, a less brittle failure profile than the T300 pins is observed.

Keywords
Z-Pinning, Laminated Composite Materials, Through-Thickness Reinforcement, Glass Fibre

Published online 11/8/2026, 4 pages
Copyright © 2026 by the author(s)
Published under license by Materials Research Forum LLC., Millersville PA, USA

Citation: Romain RUTAR, Luiz KAWASHITA, Eduardo SANTANA DE VEGA, Christophe BOUVET, Bruno CASTANIÉ, Stephen R HALLETT, Novel Glass Fibre Z-Pins to Improve the Delamination Bridging Performance of Laminated Composite Materials, Materials Research Proceedings, Vol. 73, pp 166-169, 2026

DOI: https://doi.org/10.21741/9781644904459-33

The article was published as article 33 of the book Mechanics of Advanced Materials and Structures

Content from this work may be used under the terms of the Creative Commons Attribution 3.0 license. Any further distribution of this work must maintain attribution to the author(s) and the title of the work, journal citation and DOI.

References
[1] D. D. R. Cartié, G. Dell’Anno, E. Poulin, et I. K. Partridge, « 3D reinforcement of stiffener-to-skin T-joints by Z-pinning and tufting », Engineering Fracture Mechanics, vol. 73, no 16, p. 2532‑2540, nov. 2006. https://doi.org/10.1016/j.engfracmech.2006.06.012
[2] J. Toral Vazquez, B. Castanié, J.-J. Barrau, et N. Swiergiel, « Multi-level analysis of low-cost Z-pinned composite joints Part 1: Single Z-pin behaviour », Composites Part A: Applied Science and Manufacturing, vol. 42, no 12, p. 2070‑2081, déc. 2011. https://doi.org/10.1016/j.compositesa.2011.09.018
[3] E. Santana De Vega, G. Allegri, B. Zhang, I. Hamerton, et S. R. Hallett, « Pseudo-ductile behaviour of fibrous composite Z-pins », Composites Part A: Applied Science and Manufacturing, vol. 178, p. 108009, mars 2024. https://doi.org/10.1016/j.compositesa.2024.108009
[4] A. Knopp et G. Scharr, « Effect of z-pin surface treatment on delamination and debonding properties of z-pinned composite laminates », J Mater Sci, vol. 49, no 4, p. 1674‑1683, févr. 2014. https://doi.org/10.1007/s10853-013-7851-2
[5] F. Pegorin, K. Pingkarawat, S. Daynes, et A. P. Mouritz, « Influence of z-pin length on the delamination fracture toughness and fatigue resistance of pinned composites », Composites Part B: Engineering, vol. 78, p. 298‑307, sept. 2015. https://doi.org/10.1016/j.compositesb.2015.03.093
[6] B. M’membe, M. Yasaee, S. R. Hallett, et I. K. Partridge, « Effective use of metallic Z-pins for composites’ through-thickness reinforcement », Composites Science and Technology, vol. 175, p. 77‑84, mai 2019. https://doi.org/10.1016/j.compscitech.2019.02.024
[7] M. Yasaee, L. Bigg, G. Mohamed, et S. R. Hallett, « Influence of Z-pin embedded length on the interlaminar traction response of multi-directional composite laminates », Materials & Design, vol. 115, p. 26‑36, févr. 2017. https://doi.org/10.1016/j.matdes.2016.11.025