The Effect of TVAC Cycles on Mechanical Properties of Coated AA7075 via Hard Anodization and Pulsed Laser Deposition: A Comparative Study for Space Applications
Emanuele Nicolò PIZZO, Luca GIULIANI, Andrea SEMERARO, Andrea RAYMOND, Federico PICCAGLI, Diego SCACCABAROZZI, Nora LECIS, Chiara MARTINA, Fabio DI FONZO, Nicola CEFIS
Abstract. In the space environment, aluminum alloys used in structural applications are exposed to severe conditions such as debris impacts and extreme temperature fluctuations. These phenomena can significantly compromise surface integrity, leading to increased wear, reduced mechanical performance, and premature failure of components. To address these challenges, various surface treatments have been developed to form protective oxide films on aluminum surfaces. Hard anodization is the traditional and widely adopted method, producing thick, hard and columnar aluminum oxide through an electrochemical reaction. Recently, Pulsed Laser Deposition (PLD) has emerged as a potential alternative, offering the possibility of depositing dense, uniform thin films with strong adhesion to the substrate. The aim of this work is to assess the reliability of both coating techniques when samples are subjected to TVAC cycling. To achieve this objective, AA7075-T6 coated samples underwent both thermal cycling in vacuum and tribo-mechanical tests. To simulate the Low Earth Orbit (LEO) exposure, the environment in which the “6S CubeSat” of the PoliSpace project is subjected, a Thermal Vacuum Chamber (TVAC) was used, following “ECSS-E-ST-10-03C” standard. By maintaining a high vacuum level, the samples underwent a specifically designed thermal cycle, with the maximum and minimum temperatures chosen based on the thermal study of the cited project. These temperatures were the ones at which premature failure of some components of the CubeSat was observed [1]. Subsequently, the mechanical behaviour of the coatings was characterized both before and after TVAC exposure, focusing on properties critical to in-orbit durability. Vickers and Berkovich tests were conducted to monitor changes in surface hardness for hard anodized and PLD coatings, respectively. Vickers micro-hardness tests followed the procedures outlined in “ISO-4516-2002”, while Berkovich nano-hardness tests were selected for the PLD coatings due to their limited thickness. The friction coefficient and coating wear must be considered for the CubeSat rails, as these components are critical for the satellite’s release from the rocket’s storage chamber. To assess the performance of our coatings in relation to these factors, a pin-on-disk wear test was conducted under dry conditions. Coating adhesion, a crucial factor for the stability of space structures in the presence of sliding space debris, was evaluated through scratch tests following “ASTM-C-1624-05”. These tests provided insights into interface stability, coating adhesion under increasing applied load, and the failure mechanism. A quasi-static load ramp was applied to avoid impact-like loading conditions.
Keywords
Hard Anodization, PLD, Space Applications, Aluminium, TVAC, Mechanical Performance, Tribological Tests
Published online 7/20/2026, 5 pages
Copyright © 2026 by the author(s)
Published under license by Materials Research Forum LLC., Millersville PA, USA
Citation: Emanuele Nicolò PIZZO, Luca GIULIANI, Andrea SEMERARO, Andrea RAYMOND, Federico PICCAGLI, Diego SCACCABAROZZI, Nora LECIS, Chiara MARTINA, Fabio DI FONZO, Nicola CEFIS, The Effect of TVAC Cycles on Mechanical Properties of Coated AA7075 via Hard Anodization and Pulsed Laser Deposition: A Comparative Study for Space Applications, Materials Research Proceedings, Vol. 69, pp 1397-1401, 2026
DOI: https://doi.org/10.21741/9781644904251-244
The article was published as article 244 of the book CEAS – AIDAA Conference 2025
Content from this work may be used under the terms of the Creative Commons Attribution 3.0 license. Any further distribution of this work must maintain attribution to the author(s) and the title of the work, journal citation and DOI.
References
[1] Botti, F., Dowell, M., Raymond, A., Mazzotti, L., Piunti, M., Bianchini, G., Bernasconi, L., Raveane, M., Biella, A., Maconi, E., Fascendini, D., Festa, L., Serlini, M., Platano, G., Sportelli, L., Curti, G., Vescovi, P., Malandra, A., Bedoya, J., … Schembri, F. (2024). Structural and Thermal Model testing campaign of a 1U CubeSat. https://doi.org/10.52202/078376-0001
[2] Lerner, L. M. (2010). Hard anodising of aerospace aluminium alloys. Transactions of the Institute of Metal Finishing, 88(1), 21–24. https://doi.org/10.1179/174591909X12614823458038
[3] Garc ́ıa Ferr ́e, F., Bertarelli, E., Chiodoni, A., Carnelli, D., Gastaldi, D., Vena, P., Beghi, M. G., & di Fonzo, F. (2013). The mechanical properties of a nanocrystalline Al2O3/a-Al2O3 composite coating measured by nanoindentation and Brillouin spectroscopy. Acta Materialia, 61(7), 2662–2670. https://doi.org/10.1016/j.actamat.2013.01.050
[4] Sarhan, A. A. D., Zalnezhad, E., & Hamdi, M. (2013). The influence of higher surface hardness on fretting fatigue life of hard anodized aerospace AL7075-T6 alloy. Materials Science and Engineering: A, 560, 377–387. https://doi.org/10.1016/j.msea.2012.09.082
[5] SERT, Y. (2020). Determining Optimum Anodic Oxidation Parameters for Hardness and Wear Properties of AA7075-T6 Alloys Using Taguchi Design. Brilliant Engineering, 2(1), 10–18. https://doi.org/10.36937/ben.2021.001.003